Austenitic & Super Austenitics Steels

TP 904L • UNS N08904 • 1.4539
  • Application

UNS NO8904, commonly known as 904L, is a low carbon high alloy austenitic stainless steel which is widely used in applications where the corrosion properties of AISI 316L and AISI 317L are not adequate.

The addition of copper to this grade gives it corrosion resistant properties superior to the conventional chrome nickel stainless steels, in particular to sulphuric, phosphoric and acetic acids. However, there is limited use with hydrochloric acids. It also has a high resistance to pitting in chloride solutions, a high resistance to both crevice and stress corrosion cracking. Alloy 904L performs better than other austenitic stainless steels due to the higher alloying of nickel and molybdenum. The grade is non-magnetic in all conditions and has excellent formability and weldability. The austenitic structure also gives this grade excellent toughness, even down to cryogenic temperatures The high chromium content promotes and maintains a passive film which protects the material in many corrosive environments. 904L has a greater resistance to precipitation of ferrite and sigma phases on cooling and welding than other stainless steels containing molybdenum such as 316L and 317L. There is no risk of intercrystalline corrosion on cooling or welding due to the low carbon content. Its maximum service temperature is at 450°C. This grade is particularly useful in control and instrumentation tubing applications where 316 and 317L are not suitable.

  • Typical manufacturing specifications

ASTM A213, ASTM A269, ASTM A312, ASTM A632 Also individual customer specifications.

  • Industries predominantly using this grade

Condensers, Heat exchangers, Control acd instrumentation Chemical processes, Oil and gas, Pharmaceutical etc.

Manufacturer of seamless tubes and pipes

Technical Data

Chemical composition(% by Weight)

Element

C

Mn

P

S

Si

Ni

Cr

Mo

N

Cu

Minimum

-

-

-

-

-

23.0

19.0

4.0

-

1.00

Maximum

0.020

2.00

0.040

0.030

1.00

28.0

23.0

5.0

0.10

2.00

Mechanical Properties

Specifications(Tubing, Annealed) Actual data
Tensile Rm
71
ksi (min.)
82 ~ 98
ksi
Tensile Rm
490
MPa (min.)
570 ~ 680
MPa
Yield (R.p. 0.2%)
31
ksi (min.)
40 ~ 53
ksi
Yield (R.p. 0.2%)
215
MPa (min.)
280 ~ 370
MPa
Elongation
35
% (min.)
41 ~ 48
%